A vessel is usually specified by a temperature and a pressure. The mechanism that destroys it is decided by what is in the gas, and that is a feedstock question long before it is an engineering one.
Ask why a material was chosen for a hot gas path and the answer usually starts with a maximum continuous service temperature. That number is real and it matters, and on its own it says almost nothing about how long the component will last. A metal that is perfectly happy at a given temperature in clean oxidising conditions can fail in months at a much lower temperature if the gas carries chlorides.
This is the gap that opens early in a project and widens quietly. The material selection is made when the process is still a series of assumptions, and it is made against a design basis that describes a feedstock as though it were one thing. A waste-derived feedstock is not one thing. It is a range, and the chemistry at the extremes is what the metal will actually see.
High temperature damage and low temperature damage are different problems with different remedies, and a plant contains both.
At the hot end, the attack is chemical and it is driven by what the gas carries. Oxidation at the surface is expected and can be designed for. The dangerous variants arrive with contaminants: alkali metals and chlorides that form low melting point compounds on the surface, sulphur species that interfere with the protective oxide layer, and deposits that hold those compounds against the metal instead of letting them pass. The result is not a uniform thinning that an allowance can absorb. It is localised loss, and it happens where the deposit sits.
At the cold end, and this is the part that surprises people, the mechanism is often aqueous. Anywhere the gas temperature drops below the condensation point of water or of an acid, liquid forms on a surface that the design treated as dry. Chlorides concentrate in that liquid, and chloride attack on stainless steel is not a slow problem. It pits, and in the presence of stress it cracks, and both of those can go from invisible to structural in a short period. A plant that is designed for hot gas and then operated at lower load spends more time than expected in this regime.
Between the two sits the whole length of the downstream path, and the conditions vary along it. Material selection is therefore not a single decision. It is a series of local decisions, and the failure will happen at whichever location was analysed least carefully.
The practical consequence is that every material choice embeds an assumption about what will be in the gas, and most projects record that assumption in the process description rather than in the material specification. The two documents then drift apart.
That drift has a cost. A plant commissioned on a clean feedstock and later fed a wider one does not fail immediately; it fails earlier than its replacement schedule expected, and the failure appears at the hottest or coldest point rather than in the middle. When that happens, the material is usually blamed and the feedstock change is forgotten, and the replacement is specified from the same original assumption.
The useful discipline is to write the assumption down where it can be tested. If the alloy was chosen because chlorides will stay below a given level in the gas, then that level is a control limit, not a design footnote. It belongs in the operating envelope, in the feedstock acceptance criteria and in whatever the plant measures continuously. A materials decision that is not expressed as a limit on the gas is an assumption nobody can defend three years later.
The first honest difficulty is that the material is usually bought before the feedstock is fully characterised. In a waste project the feedstock picture firms up late, and the long-lead items are ordered early, so the sequence is against you. Alloy plate is not re-specified at the end of a project, and refusing to commit until the analysis is complete can cost more in programme than it saves in maintenance.
The second is that the best material for the service is not always the best material for the job. Some alloys that resist the chemistry are difficult to weld, hard to form, or available only in a limited range of thicknesses and lead times. A specification that ignores fabrication will be quietly substituted during construction, and a substitution made under programme pressure is a materials decision taken by somebody who was not in the original conversation.
The third is that over-specifying is not free and not always safer. Buying a highly alloyed material throughout costs capital, delays delivery and sometimes creates its own problems, because higher alloys are not uniformly better at every mechanism. There is also a behavioural trap in corrosion allowances. A design that adds thickness and assumes uniform loss will be right about the average and wrong about the location, because the failures are local.
The fourth, and the one that matters most in practice, is that corrosion failures are rarely in the plate. They are at welds, heat affected zones, expansion joints, bellows, supports and the places where two materials meet. Those locations are where the fabrication quality and the local conditions both vary, and they are the hardest to inspect. No amount of alloy selection compensates for a joint that was not made well or a detail that traps liquid.
And the question that decides the rest: what is the replacement interval assumed for each of these components, and who is responsible when the material reaches the end of its life earlier than that?